Ceramic shapes

Service limit: up to 1,650 °CUsed in 3 furnace types

Ceramic riser tubes of high-purity alumina or silicon nitride transport the melt from the crucible into the die. They must withstand extreme thermal shock loading, since with every casting cycle hot melt rises and falls back again. Depending on alloy and cycle time, the service life varies between 2,000 and 5,000 shots. Timely replacement prevents fractures and uncontrolled escape of melt.

Properties

Thermal shock resistanceVery good
Erosion resistanceVery good
Chemical purityOutstanding
Dimensional accuracyOutstanding

Advantages

  • High thermal shock resistance for cyclic operation
  • Chemically inert towards aluminium melt
  • Precise dimensional accuracy for a gas-tight connection

A materials question?

Which material belongs where is decided by the plant, not the catalogue. We advise and install — free initial consultation.

CallSend enquiry

Your privacy matters to us.

We use cookies and similar technologies to ensure that our website functions properly and to analyse how our content is used. In the settings you can choose which cookies you wish to allow. Privacy policy